China OEM Customized Forging Steel Drive Shaft Eccentric Shaft Wind Power Main Flange Shaft supplier

Product Description

Supply Ability

Supply Ability
500 Metric Ton/Metric Tons per Month

Packaging & delivery

Packaging Details
Standard seaway packing or as client required.
Port
HangZhou

 

HSS M42 Steel Bright Round Bar :       

 

Grade:

AISI M42, DIN 1.3247, ASTM A600, JIS SKH59, GB W2Mo9Cr4VCo8

 

chemical composition%

C

Si

Mn

P

S

Cr

V

W

Mo

Co

1.00~1.15

≥0.65

≥0.40

≥0.030

≥0.030

3.50~4.50

0.95~1.35

1.15~1.85

9.0~10.0

7.50~8.50

 

Anneal temperature: 860-880

Relief annealing temperature: 720-760

Hardening temperature: 1160-1190

Hardening medium: salt bath under 600,aslo use oil cooling or air cooling

Normal temper temperation: 540-560
RC Rockwell Hardness after hardening and temper: 66-68

 

Characteristic:

High performance tungsten-molybdenum high speed steel, Excellent performance of hardness, red hardness, thermoplasticity, machinability. Only weak in toughness.

 

M-42 is a molybdenum-chromium-vanadium-tungsten high speed steel alloy with an additional 8% cobalt. It is widely used in metal manufacturing because of its superior red-hardness as compared to more conventional high speed steels, allowing for shorter cycle times in production environments due to higher cutting speeds or from the increase in time between tool changes. M-42 is also less prone to chipping when used for interrupted cuts and cost less when compared to the same tool made of carbide.

 

 

 

Application:

used in various of complicated tools,e.g pricision broaches, form cutter,professional lathe tool and various high hardness tools as below:

 

Broaches Cold Extrusion Punches Counter Bores
End Mills Form Cutters Keyway Cutters
Planer Tools Reamers Roll Turning Tools
Shaving Tools Taps Twist Drills

 

Report Suspicious Activity!

 

Overview

Essential details

Steel Grade:

W2Mo9Cr4VCo8

Standard:

AiSi, ASTM, bs, DIN, GB, JIS

Place of Origin:

China

Model Number:

M42

Technique:

Cold Drawn

Application:

Tool Steel Bar

Alloy Or Not:

Is Alloy

Special Use:

Mold Steel

Type:

Alloy Steel Bar

Tolerance:

0~+1mm

Processing Service:

Cutting

Grade:

W2Mo9Cr4VCo8

surface:

black or machined

type:

high speed steel

most used:

steel shaft

Supply Ability

Supply Ability
500 Metric Ton/Metric Tons per Month

Packaging & delivery

Packaging Details
Standard seaway packing or as client required.
Port
HangZhou

 

HSS M42 Steel Bright Round Bar :       

 

Grade:

AISI M42, DIN 1.3247, ASTM A600, JIS SKH59, GB W2Mo9Cr4VCo8

 

chemical composition%

C

Si

Mn

P

S

Cr

V

W

Mo

Co

1.00~1.15

≥0.65

≥0.40

≥0.030

≥0.030

3.50~4.50

0.95~1.35

1.15~1.85

9.0~10.0

7.50~8.50

 

Anneal temperature: 860-880

Relief annealing temperature: 720-760

Hardening temperature: 1160-1190

Hardening medium: salt bath under 600,aslo use oil cooling or air cooling

Normal temper temperation: 540-560
RC Rockwell Hardness after hardening and temper: 66-68

 

Characteristic:

High performance tungsten-molybdenum high speed steel, Excellent performance of hardness, red hardness, thermoplasticity, machinability. Only weak in toughness.

 

M-42 is a molybdenum-chromium-vanadium-tungsten high speed steel alloy with an additional 8% cobalt. It is widely used in metal manufacturing because of its superior red-hardness as compared to more conventional high speed steels, allowing for shorter cycle times in production environments due to higher cutting speeds or from the increase in time between tool changes. M-42 is also less prone to chipping when used for interrupted cuts and cost less when compared to the same tool made of carbide.

 

Supply Ability

Supply Ability
500 Metric Ton/Metric Tons per Month

Packaging & delivery

Packaging Details
Standard seaway packing or as client required.
Port
HangZhou

 

HSS M42 Steel Bright Round Bar :       

 

Grade:

AISI M42, DIN 1.3247, ASTM A600, JIS SKH59, GB W2Mo9Cr4VCo8

 

chemical composition%

C

Si

Mn

P

S

Cr

V

W

Mo

Co

1.00~1.15

≥0.65

≥0.40

≥0.030

≥0.030

3.50~4.50

0.95~1.35

1.15~1.85

9.0~10.0

7.50~8.50

 

Anneal temperature: 860-880

Relief annealing temperature: 720-760

Hardening temperature: 1160-1190

Hardening medium: salt bath under 600,aslo use oil cooling or air cooling

Normal temper temperation: 540-560
RC Rockwell Hardness after hardening and temper: 66-68

 

Characteristic:

High performance tungsten-molybdenum high speed steel, Excellent performance of hardness, red hardness, thermoplasticity, machinability. Only weak in toughness.

 

M-42 is a molybdenum-chromium-vanadium-tungsten high speed steel alloy with an additional 8% cobalt. It is widely used in metal manufacturing because of its superior red-hardness as compared to more conventional high speed steels, allowing for shorter cycle times in production environments due to higher cutting speeds or from the increase in time between tool changes. M-42 is also less prone to chipping when used for interrupted cuts and cost less when compared to the same tool made of carbide.

 

 

 

Application:

used in various of complicated tools,e.g pricision broaches, form cutter,professional lathe tool and various high hardness tools as below:

 

Broaches Cold Extrusion Punches Counter Bores
End Mills Form Cutters Keyway Cutters
Planer Tools Reamers Roll Turning Tools
Shaving Tools Taps Twist Drills

 

Application:

used in various of complicated tools,e.g pricision broaches, form cutter,professional lathe tool and various high hardness tools as below:

 

Broaches Cold Extrusion Punches Counter Bores
End Mills Form Cutters Keyway Cutters
Planer Tools Reamers Roll Turning Tools
Shaving Tools Taps Twist Drills

 

Products Name Carbon Steel Bar
Steel Grade Q195,Q235,Q345, 45#, S20C , SAE1571,SAE1571,SAE1045,EN8,EN19,C45,CK45,SS400 etc
Standard ASTM A 615 Gr 40/60,BSS4449 Gr460B,500B etc
Diameter 6mm-1200mm
Length 3000mm-12000mm or as client’s request
Straightness 3mm/M max
Tolerance +0.5mm/-0(dia),+5mm/-0(L)
MOQ 1 tons
Heat treatment Normalized / Annealed / Quenched / tempered
Surface black,mill,polished,brush,etc
Test Ultrasonic test according to SEP 1921-84 G3 C/c
HS Code 72210000,72221100,72222000,72223000
Application Widely used in construction industry for reinforcing concret(Express way; office building, Bridge etc) Trasportation By sea(20′ 40′ container), parts of larger cross-sections, crankshafts, gears.
Trade Term FOB, CFR, CIF
Payment 30% advance by T\T; Balance pay before the shipment against shipping documents or irrevocable LC at sight
Packaging Export standard, seaworthy
Delivery time 10-20days after confirmed order
Loading port ZheJiang port , ZheJiang port or as client’s request
Container size 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High) 
40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High)  
40ft HC:12032mm(Length)x2352mm(Width)x2698mm(High)
Item Type Diameter (MM) Length 
Round Bar  8~400 6/9/12m or follow client’s requirment.
Steel Wire Rod  5.5~34 Coil
Steel Rebar 5.5~40 Cut to length or Coil
Remark

We are sure that we can establish good relationships, feel free to contact us We are sure to satisfy you with our profeessional information.
Top quality, best price and efficient service

Don’t hesitate to contact us.

Product Description

Standard

JIS / ASTM / GB / DIN / EN /AISI

Material

Cr12mov  H13  SKD11  SKD6 D2 DC53 7CrSiMnMoV  1.2344 1.2379 4Cr13 P20 2738 B40  5CrNiMo  5CrMnMo

Diameter

80-400mm

Length

400-6000mm or be required

Technique

Hot Rolled / Forged / Cold Drawn

MOQ

5tons

Packing

In bundles tied with steel stripes or as request

Payment terms

L/C at sight or T/T (30% as deposit)

Delivery time

Usually 7-15 dyas, or CZPT negotiation

Samples

Free samples are provided but the fright is paid by the buyer

Type: Round
Standard: AISI, ASTM, DIN, JIS, GB, BS
Composition: Stainless Steel Scrap
Technique: Hot Rolled
Shape: Bar
Surface Treatment: Polished
Samples:
US$ 5/kg
1 kg(Min.Order)

|
Request Sample

Customization:
Available

|

Customized Request

air-compressor

How to Replace the Drive Shaft

Several different functions in a vehicle are critical to its functioning, but the driveshaft is probably the part that needs to be understood the most. A damaged or damaged driveshaft can damage many other auto parts. This article will explain how this component works and some of the signs that it may need repair. This article is for the average person who wants to fix their car on their own but may not be familiar with mechanical repairs or even driveshaft mechanics. You can click the link below for more information.

Repair damaged driveshafts

If you own a car, you should know that the driveshaft is an integral part of the vehicle’s driveline. They ensure efficient transmission of power from the engine to the wheels and drive. However, if your driveshaft is damaged or cracked, your vehicle will not function properly. To keep your car safe and running at peak efficiency, you should have it repaired as soon as possible. Here are some simple steps to replace the drive shaft.
First, diagnose the cause of the drive shaft damage. If your car is making unusual noises, the driveshaft may be damaged. This is because worn bushings and bearings support the drive shaft. Therefore, the rotation of the drive shaft is affected. The noise will be squeaks, dings or rattles. Once the problem has been diagnosed, it is time to repair the damaged drive shaft.
Professionals can repair your driveshaft at relatively low cost. Costs vary depending on the type of drive shaft and its condition. Axle repairs can range from $300 to $1,000. Labor is usually only around $200. A simple repair can cost between $150 and $1700. You’ll save hundreds of dollars if you’re able to fix the problem yourself. You may need to spend a few more hours educating yourself about the problem before handing it over to a professional for proper diagnosis and repair.
The cost of repairing a damaged driveshaft varies by model and manufacturer. It can cost as much as $2,000 depending on parts and labor. While labor costs can vary, parts and labor are typically around $70. On average, a damaged driveshaft repair costs between $400 and $600. However, these parts can be more expensive than that. If you don’t want to spend money on unnecessarily expensive repairs, you may need to pay a little more.
air-compressor

Learn how drive shafts work

While a car engine may be one of the most complex components in your vehicle, the driveshaft has an equally important job. The driveshaft transmits the power of the engine to the wheels, turning the wheels and making the vehicle move. Driveshaft torque refers to the force associated with rotational motion. Drive shafts must be able to withstand extreme conditions or they may break. Driveshafts are not designed to bend, so understanding how they work is critical to the proper functioning of the vehicle.
The drive shaft includes many components. The CV connector is one of them. This is the last stop before the wheels spin. CV joints are also known as “doughnut” joints. The CV joint helps balance the load on the driveshaft, the final stop between the engine and the final drive assembly. Finally, the axle is a single rotating shaft that transmits power from the final drive assembly to the wheels.
Different types of drive shafts have different numbers of joints. They transmit torque from the engine to the wheels and must accommodate differences in length and angle. The drive shaft of a front-wheel drive vehicle usually includes a connecting shaft, an inner constant velocity joint and an outer fixed joint. They also have anti-lock system rings and torsional dampers to help them run smoothly. This guide will help you understand the basics of driveshafts and keep your car in good shape.
The CV joint is the heart of the driveshaft, it enables the wheels of the car to move at a constant speed. The connector also helps transmit power efficiently. You can learn more about CV joint driveshafts by looking at the top 3 driveshaft questions
The U-joint on the intermediate shaft may be worn or damaged. Small deviations in these joints can cause slight vibrations and wobble. Over time, these vibrations can wear out drivetrain components, including U-joints and differential seals. Additional wear on the center support bearing is also expected. If your driveshaft is leaking oil, the next step is to check your transmission.
The drive shaft is an important part of the car. They transmit power from the engine to the transmission. They also connect the axles and CV joints. When these components are in good condition, they transmit power to the wheels. If you find them loose or stuck, it can cause the vehicle to bounce. To ensure proper torque transfer, your car needs to stay on the road. While rough roads are normal, bumps and bumps are common.
air-compressor

Common signs of damaged driveshafts

If your vehicle vibrates heavily underneath, you may be dealing with a faulty propshaft. This issue limits your overall control of the vehicle and cannot be ignored. If you hear this noise frequently, the problem may be the cause and should be diagnosed as soon as possible. Here are some common symptoms of a damaged driveshaft. If you experience this noise while driving, you should have your vehicle inspected by a mechanic.
A clanging sound can also be one of the signs of a damaged driveshaft. A ding may be a sign of a faulty U-joint or center bearing. This can also be a symptom of worn center bearings. To keep your vehicle safe and functioning properly, it is best to have your driveshaft inspected by a certified mechanic. This can prevent serious damage to your car.
A worn drive shaft can cause difficulty turning, which can be a major safety issue. Fortunately, there are many ways to tell if your driveshaft needs service. The first thing you can do is check the u-joint itself. If it moves too much or too little in any direction, it probably means your driveshaft is faulty. Also, rust on the bearing cap seals may indicate a faulty drive shaft.
The next time your car rattles, it might be time for a mechanic to check it out. Whether your vehicle has a manual or automatic transmission, the driveshaft plays an important role in your vehicle’s performance. When one or both driveshafts fail, it can make the vehicle unsafe or impossible to drive. Therefore, you should have your car inspected by a mechanic as soon as possible to prevent further problems.
Your vehicle should also be regularly lubricated with grease and chain to prevent corrosion. This will prevent grease from escaping and causing dirt and grease to build up. Another common sign is a dirty driveshaft. Make sure your phone is free of debris and in good condition. Finally, make sure the driveshaft chain and cover are in place. In most cases, if you notice any of these common symptoms, your vehicle’s driveshaft should be replaced.
Other signs of a damaged driveshaft include uneven wheel rotation, difficulty turning the car, and increased drag when trying to turn. A worn U-joint also inhibits the ability of the steering wheel to turn, making it more difficult to turn. Another sign of a faulty driveshaft is the shuddering noise the car makes when accelerating. Vehicles with damaged driveshafts should be inspected as soon as possible to avoid costly repairs.

China OEM Customized Forging Steel Drive Shaft Eccentric Shaft Wind Power Main Flange Shaft   supplier China OEM Customized Forging Steel Drive Shaft Eccentric Shaft Wind Power Main Flange Shaft   supplier
editor by CX 2023-06-12